Return to PREVIOUS Page
Go to the NEXT Page

Neodymium

Density 7.00 g/cm3
Thermal Conductivity @ 25oC 0.031 cal/(s/cm/oC)
Specific Heat @ 25oC 0.045 cal/g
Heat of Fusion 1.70 kcal/g-atom
Latent Heat of Fusion kcal/g-mole
Heat of Vaporization 69 kcal/g-atom
Latent Heat of Vaporization kcal/g-atom
Atomic Volume 20.6 W/D
First Ionizaton Energy 145 kcal/g-mole
Electronegativity 1.2 Paulings
Covalent Radius 1.64 Angstroms
Brinell Hardness  
Mohs Hardness @ 20oC  
Vickers Hardness @ 20oC  
Linear CTE @ 20oC x 10-6
Electrical Resistivity @ 298oK 64.3 mohm/cm
Electrical Conductance mohm-1
Crystal Structure Hexagonal
Curie Temperature oC
Modulus of Elasticity kg/mm2
Youngs Modulus psi
Thermal Neutron Cross-section 46 barnes/atom
Magnetic Moment 3.3 Bohr magnetons
Magnetic Succeptibility @ 18oC 5.65 x 10-9 emu/mole
Tensile Strength 24700 psi
Yield Strength 23900 psi
Electron Work Function  
Vapor Pressure @ 25 oC m
Poisson Ratio  
Shear Modulus  
Critical Temperature oC
Transformation Temperature 855oC
Critical Pressure atm
Standard Electrode Potential +2.24 Volts
Ionization Potential eV
Compressability 3.0 x 10-6 /atm
Thermionic Work Function eV
Debye Temperature oK
Yield Point psi
Hall Consatant x 10-13 (ohm/cm)/gauss
Lattice Constant 10-8 cm